Aqueous Extraction
Quantitative gravimetric testing measures the weight reduction observed when unbleached flax materials undergo hot aqueous washing without aggressive chemical reagents. Designated across finishing records as water scouring loss, the metric quantifies the dissolution of water-soluble pectins, dirt particles, free monosaccharides and residual retting liquor salts. Technicians boil conditioned specimens in distilled water, rinse them thoroughly, and dry them to constant weight in an analytical drying oven.
The calculation expresses dissolved mass as a percentage of initial dry substance. Extraction procedures conclude when wash water exhibits neutral turbidity.
Boiling Preparation
Textile wet processing operations monitor this mass reduction to calibrate the intensity of subsequent caustic scouring and bleaching stages. Flax fibres contain non-cellulosic constituents that dissolve readily in neutral hot water, whereas stubborn waxes and lignins require sodium hydroxide and emulsifiers. Measuring the initial water scouring loss allows finishing managers to predict how much chemical reagent the grey cloth will consume during pressurized kier boiling or open-width continuous scouring.
If high fractions of soluble material enter alkaline processing tanks directly, bath chemicals deplete prematurely, leaving residual waxes on yarn surfaces that inhibit dye penetration. Finishing plants in Jiangsu and Zhejiang record initial hot water solubility on grey fabric lot receipts before releasing rolls to singeing and desizing ranges. Process adjustments based on these gravimetric figures ensure consistent bath concentrations and prevent uneven pale patches during package or piece dyeing.
Desizing Threshold
Purchasing specifications and processing guidelines stipulate clear boundaries for pre-scour weight removal to differentiate natural gum wash-off from chemical sizing extraction. Normal grey linen goods exhibit a clean water extraction loss between two and five percent, whereas fabric carrying starch or polyvinyl alcohol sizing yields significantly higher figures. Quality testing laboratories cite GB/T 5889 when distinguishing soluble bast gum fractions from synthetic sizing formulations applied before loom processing.
Inspection certificates report both aqueous extraction loss and total chemical desize loss to verify that fabric mills applied correct yarn lubricants. Conformance dockets validate fabric suitability before rolls proceed to commercial garment manufacturing.