Polymer Rigidity
Mechanical failure of warp yarns during weaving often stems from a loss of flexibility caused by the improper application of protective starches. Sizing embrittlement occurs when the coating intended to protect the yarn becomes too hard or lacks the necessary humectants to remain pliable. This condition leads to high breakage rates as the yarn passes through the heddles and reeds of the loom.
Mills monitor the moisture content and chemical composition of the size mix to prevent this defect. The state of the yarn is assessed immediately before the weaving process begins.
Desiccation Effect
Starch molecules form a protective film around the linen fibre, but rapid drying at high temperatures can cause the polymer chains to crystallize too tightly. When sizing embrittlement sets in, the yarn loses its ability to elongate under the sudden tension of the shed opening. Natural flax already possesses low elasticity, and a brittle size layer removes the final margin of flexibility required for high-speed industrial weaving.
Technicians test the bending stiffness of the treated yarn using a standard cantilever test or a simple snap-back observation. Adjusting the concentration of softeners such as tallow or synthetic waxes in the size box helps maintain a supple film. If the drying cylinders are set too high, the internal moisture of the yarn drops below the critical level needed for structural integrity.
Weaving Failure
Looms operating with brittle warp yarns show an increase in micro-cracks and surface hairiness in the finished fabric. Sizing embrittlement prevents the smooth movement of the shuttle or rapier through the warp. The resulting cloth often fails the final tensile strength test required by the buyer.