Linear Density Procedure
Direct physical sectioning isolates precise lengths of processed fibre strands to determine linear density through mass measurement. Within flax fibre evaluation, cut length gravimetry measures the average mass per unit length of hackled flax or sliver strands by cutting bundle specimens to a fixed length using a multi-blade cutter. The ratio of total weighed mass to total cut length yields the linear density in tex or decitex.
This method provides absolute linear density values without relying on indirect airflow or optical calibration.
Specimen Preparation Method
Tensioning frames hold fibre bundles straight without stretching individual filaments before cutting blades descend across the sample bed. Variable crimp or residual waviness causes specimen length distortion, introducing systematic error into mass calculations. Precise sample alignment prevents angled cutting that would increase individual segment length beyond nominal specifications.
After cutting, operators transfer the segment bundles onto analytical balances using fine tweezers to avoid oil contamination from skin contact. Cut length gravimetry relies on uniform sample count per batch, requiring manual counting or calibrated bundle division before mass determination. Repeated weighings under controlled humidity ensure accurate linear density values.
Yarn Spinning Limit
Spinning limit calculations rely on fine fibre linear density to predict minimum achievable yarn count without thread breaks. Coarse bundles reduce spinning limits and lower yarn uniformity.