Edge Reinforcement
Sacrificial narrow bands formed outside the primary fabric boundary provide temporary grip for rapier insertion clamps and catch yarn ends before cutter trimming. An auxiliary selvedge stabilises the outer warp ends against heavy beat-up impact on shuttleless rapier machinery. Rigid wet-spun flax yarn displays poor elasticity under cyclic shedding strain, which makes peripheral support indispensable during high-speed cloth formation.
Without this temporary perimeter band, uneven tension drops propagate into the usable linen panel, causing dropped picks and loose edge tension across the outer centimetres of the beam. Mill inspection sheets log the occurrence of ruptured sacrificial ends during piece changes.
Loom Setting
Heald shafts operating on independent cam motions control the auxiliary selvedge yarns outside the reed width allocated to the sellable piece. These secondary harnesses raise and lower polyester or bast core yarns in plain interlacing orders, locking the inserted weft firmly in place before the mechanical cutter strokes. Flax weft yarns exhibit natural irregularities in diameter that generate variable friction against edge needles.
Stable grip demands higher crossing tension than the body cloth requires. Mechanical leno devices or independent binding units frequently maintain the hold on flax filling tails, guaranteeing uniform cut margins prior to cloth take-up roll winding.
Trim Disposition
Cutter blades sever the auxiliary selvedge immediately forward of the fell line, directing the detached ribbon down suction tubes or into scrap hoppers beside the take-up roll. The resulting waste band contains contaminated or broken linen picks entangled with synthetic binder ends, preventing direct wet-spinning re-processing without mechanical sorting. Mill cost accounting isolates this sacrificial waste as a continuous yield loss against initial beam calculations.
Buyer purchase specifications define the usable cloth width strictly inside the line of severance, rejecting deliveries where residual catch bands or pulled binding loops encroach upon the primary selvage pins. Regular micrometer checks verify uniform edge clearance across every batch.