Repeating Pattern
Physical flaws that appear at regular intervals along the length of a fabric roll due to mechanical failure in the loom or finishing equipment. These continuous running defects appear as stripes, streaks, physical holes or structural gaps that persist for several meters. Identification usually occurs during the final inspection on the scrolling table.
Because the flaw is consistent, it renders the affected section of linen unusable for standard garment panels, which leads to heavy material waste.
Mechanical Cause
Worn rollers or damaged needles typically trigger these issues during the high speed weaving process. When a reed becomes bent or a lubricating pump leaks, continuous running defects occur across the entire production run until the machinery is stopped for repair. Regular maintenance checks aim to catch these mechanical drifts before they ruin a whole batch.
Correcting the alignment of the take-up motion often solves the problem.
Grading Penalty
Heavy point deductions apply when a flaw repeats without interruption throughout a piece of cloth. Most quality standards dictate that continuous running defects result in the immediate classification of the roll as second quality or scrap. This rule prevents the mill from shipping fabric that would lead to mass failures in the cutting room.