Spinning Interruption
Yarn manufacturing processes experience interruptions when the tensile stress on the spinning strand exceeds its structural strength. This failure event, known as ring frame breakage, occurs on the spinning frame when the wet-spun flax yarn snaps before being wound onto the bobbin. The frequency of these events is recorded as a primary performance indicator of the mill’s spinning efficiency.
Tension Variation
Wet spinning of flax requires high yarn tension to wind the yarn tightly onto the wooden bobbins. If the drafting ratch or the traveler weight is incorrect, the yarn suffers from frequent ring frame breakage, which forces the operator to stop the spindle and piece the yarn together. Each piecing creates a knot or a thick spot in the yarn that reduces its quality grade on the final yarn inspection sheet.
The mill’s spinning supervisor tracks the break rate per thousand spindles to maintain yarn consistency. High break rates lead to yarn that fails the strength tests demanded by downstream processing.
Spindle Balance
Wear on the ring or the traveler can create uneven resistance that increases the mechanical stress on the spun yarn. Regular maintenance of the ring rail assembly is necessary to reduce the tension spikes that trigger these breaks. This upkeep ensures a continuous and high-volume yarn production.