Chemical Scouring
Chemical pre-treatment removes non-cellulosic impurities from flax textiles using heated caustic solutions. During alkaline boiling, the mill targets waxes and pectins that inhibit water absorption. The operation typically occurs in high pressure vessels to ensure total penetration of the fiber bundle.
This stage defines the base whiteness and wettability of the finished linen cloth.
Pectin Degradation
Caustic soda reacts with the acidic groups in the pectin chains to dissolve the glue holding the fiber bundles together. If the temperature or concentration is insufficient, the alkaline boiling fails to strip the hard shives from the fabric surface. Residual lignin remains as dark spots that interfere with subsequent bleaching cycles.
Proper control of the liquor ratio prevents the uneven concentration of chemicals.
Finishing Preparation
Successful execution results in a substrate that allows dyes and finishing agents to move deep into the crystalline structure of the cellulose. A fabric that skips or shortens the alkaline boiling period often exhibits poor color fastness and a stiff hand feel (a characteristic known as harshness in the trade). Chinese mill standards often specify the weight loss percentage after scouring as a measure of treatment intensity.
When the weight loss exceeds the expected range, the mechanical strength of the flax fibers might be compromised. Solvent extraction verifies the residual wax content. Consistency in this chemical bath is the primary determinant of batch to batch color uniformity in large scale linen production.