Spectral Peak
A sharp, narrow spike on a yarn mass spectrogram indicates a recurring defect in the thickness of the sliver or yarn. This phenomenon, referred to as a periodic chimney, represents a highly localized concentration of mass variation at a specific wavelength. It contrasts with the broad, random variation caused by the natural distribution of fibre lengths.
Mechanical Origin
Mechanical malfunctions such as an eccentric roller, a damaged gear tooth or a slipping belt generate these distinct peaks. The wavelength at which the spike appears is directly related to the circumference or rotational speed of the faulty component. By calculating the physical distance of the repeat, technicians can locate the specific machine part that is causing the error.
Diagnostic Consequence
Quality control systems in modern mills monitor these spectral patterns to prevent mass-production of defective yarn. If a spike exceeds the pre-set tolerance threshold, the system triggers an alarm so that the affected frame can be stopped and repaired immediately. This intervention is crucial because periodic variations can create visible Moire patterns in the finished woven fabric, which would lead to the rejection of the entire batch by the buyer.
Therefore, continuous monitoring of these peaks is a standard procedure in high-quality linen production.