Appearance Defect
Visible linear irregularities in the luster or color intensity of dyed linen fabric result from uneven chemical treatment under tension. These mercerization streaks appear when the fabric is exposed to varying concentrations of sodium hydroxide during the mercerizing process. The uneven swelling of the cellulose fibres creates different light-reflecting properties and dye absorption rates along the fabric web.
Processing Error
Mercerizing requires passing the linen fabric through a concentrated caustic soda bath while maintaining high mechanical tension to prevent shrinkage and enhance sheen. If the spray nozzles apply the chemical unevenly or if the tension rollers apply non-uniform pressure across the fabric width, the chemical reaction will vary. The fibres that receive more chemical treatment or experience higher tension swell more and absorb more dye than the less-treated sections.
This variation becomes highly visible after dyeing as long bands of darker or lighter shades running parallel to the fabric edge.
Preventive Measure
Mill operators must maintain uniform spray pressure and check roller alignment to ensure even chemical application. Continuous monitoring of bath temperature and caustic concentration also helps prevent these appearance faults. Proper maintenance of the tensioning machinery is required to produce a consistent and high-quality mercerized finish.