Quantifying Pectin Ester and Lignin Ratios in Industrial Degummed Flax
FTIR peak ratios at 1740 against 1605 cm⁻¹ paired with Klason lignin below 1.5% define the drafting boundary for spinning degummed flax on dry cotton frames.