Mass Ratio
Weight of the dry sizing material expressed as a percentage of the weight of the raw yarn defines this production value. Dry size add-on measures the amount of protective coating remaining on the flax warp after the moisture has been evaporated in the drying section of the sizing machine. Technicians record this value on the warp beam ticket to ensure the fabric meets the specifications required for the intended loom type.
Weaving Protection
Friction resistance during the weaving process depends heavily on the uniform distribution of this coating across the yarn surface. When dry size add-on falls below the target range, the flax yarn becomes vulnerable to fraying and breakage under the tension of the shedding motion. This leads to increased loom downtime and structural defects in the linen cloth.
Conversely, excessive application makes the yarn too brittle and difficult to desize during the wet finishing stages.
Consumption Calculation
Calculation of this figure involves weighing a sample of the sized yarn before and after the desizing process in a laboratory oven. The mill uses the resulting percentage to adjust the pressure of the squeeze rollers in the size box. If the concentration of the sizing liquor remains constant, the mechanical pressure of these rollers becomes the primary variable for controlling the pickup.
High precision in this measurement allows for the optimization of chemical usage and improves the quality of the woven textile.